Hi there: I have a RC 350 2015 and I noticed that the rocker molding in both side has like a wave defect exactly at the same measure, Can anyone tell me if it is normal that come with the car or is a defect, Ill appreciate your answer, my email is stenic@comcast.net
Thanks
Rick
Old 06-02-19, 12:46 AM
  #2  
CLightning
Pit Crew
 
CLightning's Avatar
 
Join Date: Jan 2006
Location: CA
Posts: 156
Received 49 Likes on 45 Posts
Default

Originally Posted by Steniriel
Hi there: I have a RC 350 2015 and I noticed that the rocker molding in both side has like a wave defect exactly at the same measure, Can anyone tell me if it is normal that come with the car or is a defect, Ill appreciate your answer, my email is stenic@comcast.net
Thanks
Rick
Normal. It almost looks like a sharp crease that runs vertically about midway along the length of the "rocker molding."
The following users liked this post:
Steniriel (06-02-19)
Old 06-02-19, 11:35 AM
  #3  
Steniriel
Driver School Candidate
Thread Starter
 
Steniriel's Avatar
 
Join Date: May 2019
Location: Florida
Posts: 19
Received 1 Like on 1 Post
Smile

Originally Posted by CLightning
Normal. It almost looks like a sharp crease that runs vertically about midway along the length of the "rocker molding."
THANK YOU VERY MUCH CLightning I bought this car used and I didn't notice after I left the dealer, and after that I was so freak out, thinking that was a damage that could complaining, I search on the internet something related to this and I couldn't find anything until now and your help, now I feel more relieved, lol. GOD BLESS YOU!
Rick
Old 06-02-19, 12:09 PM
  #4  
Steniriel
Driver School Candidate
Thread Starter
 
Steniriel's Avatar
 
Join Date: May 2019
Location: Florida
Posts: 19
Received 1 Like on 1 Post
Default

Just one question CL did you ever contact Lexus about this sharp crease? Please let me know


Thanks


Rick
Old 06-02-19, 12:29 PM
  #5  
CLightning
Pit Crew
 
CLightning's Avatar
 
Join Date: Jan 2006
Location: CA
Posts: 156
Received 49 Likes on 45 Posts
Default

No I did not because the both sides of the car look EXACTLY alike, so I knew this was normal.
The following users liked this post:
Steniriel (06-04-19)
Old 06-02-19, 07:13 PM
  #6  
Steniriel
Driver School Candidate
Thread Starter
 
Steniriel's Avatar
 
Join Date: May 2019
Location: Florida
Posts: 19
Received 1 Like on 1 Post
Thumbs up

Originally Posted by CLightning
No I did not because the both sides of the car look EXACTLY alike, so I knew this was normal.
Ok Thanks brother, have a blessed week!
Old 06-03-19, 05:10 AM
  #7  
wthrman2
Lead Lap
 
wthrman2's Avatar
 
Join Date: Oct 2014
Location: ON
Posts: 3,535
Received 3,544 Likes on 1,734 Posts
Default

Could someone post of picture of what you guys are describing? I'd be curious to see...
The following 2 users liked this post by wthrman2:
lexual_rc (03-02-20), Steniriel (06-04-19)
Old 06-03-19, 10:46 AM
  #8  
Megafast13
Instructor
 
Megafast13's Avatar
 
Join Date: Aug 2008
Location: Ohio
Posts: 1,178
Received 6 Likes on 6 Posts
Default

They all have it unfortunately. My OCD and fear kicked in when I first saw it. Must be an anchor point or bolt that slightly warps the plastic
The following users liked this post:
Steniriel (06-04-19)
Old 06-03-19, 03:52 PM
  #9  
Steniriel
Driver School Candidate
Thread Starter
 
Steniriel's Avatar
 
Join Date: May 2019
Location: Florida
Posts: 19
Received 1 Like on 1 Post
Smile lmao

Originally Posted by Megafast13
They all have it unfortunately. My OCD and fear kicked in when I first saw it. Must be an anchor point or bolt that slightly warps the plastic
lol Good one buddy, In my case sometimes I couldn't sleep,I'll try to take a pictures to show the creases in both side, Take Care!
Old 06-03-19, 03:53 PM
  #10  
Steniriel
Driver School Candidate
Thread Starter
 
Steniriel's Avatar
 
Join Date: May 2019
Location: Florida
Posts: 19
Received 1 Like on 1 Post
Default

I'll do my best to take some pictures, this coming weekend!
Old 06-03-19, 10:48 PM
  #11  
CLightning
Pit Crew
 
CLightning's Avatar
 
Join Date: Jan 2006
Location: CA
Posts: 156
Received 49 Likes on 45 Posts
Default

Originally Posted by wthrman2
Could someone post of picture of what you guys are describing? I'd be curious to see...


You can see that the defects are almost mirrored on the opposite side.
The following 2 users liked this post by CLightning:
gkcmilner (06-04-19), Steniriel (06-04-19)
Old 06-04-19, 04:02 AM
  #12  
wthrman2
Lead Lap
 
wthrman2's Avatar
 
Join Date: Oct 2014
Location: ON
Posts: 3,535
Received 3,544 Likes on 1,734 Posts
Default

I had never seen that before - I am glad you guys posted the photos so I don't freak out when I see it on mine when I pick it up. I never noticed it before but maybe on white, it is a bit less noticeable.

Much appreciated for the pics CLightning!!
The following users liked this post:
Steniriel (06-04-19)
Old 06-04-19, 10:05 AM
  #13  
Steniriel
Driver School Candidate
Thread Starter
 
Steniriel's Avatar
 
Join Date: May 2019
Location: Florida
Posts: 19
Received 1 Like on 1 Post
Smile Great Job CL!!

Originally Posted by CLightning


You can see that the defects are almost mirrored on the opposite side.
Great Job CL posting this pictures, tried to take some in my Royal Blue color but was difficult, but you did a great job, thinking because looks better in a black color, thanks again buddy, GOD BLESS YOU! One question I wonder if you have installed the OEM lip spoiler? because I had in mine car installed but after that the lid trunk don't open, maybe because the weight of the spoiler? or if you know can use a special spring or something in order to make it open completely, I'll appreciate if you can give me your advise, thanks buddy!
The following users liked this post:
lexual_rc (03-02-20)
Old 06-04-19, 01:26 PM
  #14  
sideswipe
Pole Position
 
sideswipe's Avatar
 
Join Date: Aug 2016
Location: NY
Posts: 230
Received 26 Likes on 25 Posts
Default

Originally Posted by Steniriel
Great Job CL posting this pictures, tried to take some in my Royal Blue color but was difficult, but you did a great job, thinking because looks better in a black color, thanks again buddy, GOD BLESS YOU! One question I wonder if you have installed the OEM lip spoiler? because I had in mine car installed but after that the lid trunk don't open, maybe because the weight of the spoiler? or if you know can use a special spring or something in order to make it open completely, I'll appreciate if you can give me your advise, thanks buddy!
Lip spoiler or trunk spoiler?
The following users liked this post:
Steniriel (06-04-19)
Old 06-04-19, 05:26 PM
  #15  
Steniriel
Driver School Candidate
Thread Starter
 
Steniriel's Avatar
 
Join Date: May 2019
Location: Florida
Posts: 19
Received 1 Like on 1 Post
Default

trunk spoiler, the Lexus original, thanks again